In full annealing, the hypo-eutectoid steel is heated from 30° C to 50° C above the upper critical temperature and then cooled

A)
slowly in the furnace
B)
in still air
C)
suddenly in a suitable cooling medium
D)
Any one of these

Correct Answer : Option (A) :   slowly in the furnace